이동원,최준환,임태수,김용진,Lee Dong-Won,Choi Joon-Hwan,Lim Tae-Soo,Kim Yong-Jin 한국분말야금학회 2006 한국분말재료학회지 (KPMI) Vol.13 No.3
The nanostructured cerium oxide powders were synthesized by spray thermal decomposition process for the use as the raw materials of resistive oxygen sensor. The synthesis routes consisted of 1) spray drying of water based organic solution made from cerium nitrate hydrate ($Ce(NO_3){_3}6H_2O$) and 2) heat treatment of spray dried precursor powders at $400^{\circ}C$ in air atmosphere to remove the volatile components and identically to oxidize the cerium component. The produced powders have shown the loose structure agglomerated with extremely fine cerium oxide particles with about 15 nm and very high specific surface area ($110m^2/g$). The oxygen sensitivity, n ($Log{\propto}Log (P_{O2}/P^o)^{-n}$ and the response time, $t_{90}$ measured at $600^{\circ}C$ in the sample sintered at $1000^{\circ}C$, were about 0.25 and 3 seconds, respectively, which had much higher performances than those known in micron or $100{\sim}200nm$ sized sensors.
SHS 공정에 의해 제조된 Mo<sub>x</sub>W<sub>1-x</sub>Si<sub>2</sub> 발열체의 열화메커니즘
이동원,이상헌,김용남,이성철,구상모,오종민,Lee, Dong-Won,Lee, Sang-Hun,Kim, Yong-Nam,Lee, Sung-Chul,Koo, Sang-Mo,Oh, Jong-Min 한국전기전자재료학회 2017 전기전자재료학회논문지 Vol.30 No.10
The degradation mechanism of $Mo_xW_{1-x}Si_2$ ultrahigh-temperature heating elements fabricated by self-propagating high-temperature synthesiswas investigated. The $Mo_xW_{1-x}Si_2$ specimens (with and without post-annealing) were subjected to ADTs (accelerated degradation tests) at temperatures up to $1,700^{\circ}C$ at heating rates of 3, 4, 5, 7, and $14^{\circ}C/min$. The surface loads of all the specimen heaters were increased with the increase in the target temperature. For the $Mo_xW_{1-x}Si_2$ specimens without annealing, many pores and secondary-phase particles were observed in the microstructure; the surface load increased to $23.9W/cm^2$ at $1,700^{\circ}C$, while the bending strength drastically reduced to 242 MPa. In contrast, the $Mo_xW_{1-x}Si_2$ specimens after post-annealing retained $single-Mo_xW_{1-x}Si_2$ phases and showed superior durability after the ADT. Consequently, it is thought that the formation of microcracks and coarse secondary phases during the ADT are the main causes for the degraded performance of the $Mo_xW_{1-x}Si_2$ heating elements without post-annealing.
치매(痴呆)에 관(關)한 동서의학적(東西醫學的) 비교(比較) 고찰(考察)
이동원,신길조,이원철,Lee, Dong-Weon,Shin, Gil-Jo,Lee, Won-Chul 대한한방내과학회 1995 大韓韓方內科學會誌 Vol.16 No.1
This study was done in order to investigate the etiology and pathology of dementia in the variety literature. Dementia in elderly persons(above the age of 60) mainly classfied Alzheimer disease and Cerebral vascular dementia. The results were as follows: 1. Dementia patients have abnormal mental function, who have no mental weakness but defects of memory, verbal disturbance, behavior disturbance and loss of intellectual function. 2. Dementia regard as 'me-beng(?病)', 'jeon-gwang(癲狂)', and 'heo-ro(虛勞)' in oriental medicine and the symptom is a silence with no response, mixing, a crying or a laugh, a stranger behavior and a amnesia; disturbances of speech, emotion, behavior. 3. Dementia caused by Alzheimer disease, Multi infarct dementia, Parkinson's disease, sequelae of acute CO poisoning, head injury and alcoholism(occidental medically) and the 'Dam(痰) and Damhwa(痰火), weakness of heart and spleen(心脾虛) caused by pent up anger of seven emotions(七情鬱結), the weakness of liver and kidney(肝腎不足)(oriental medically). 4. The causes of Alzheimer disease are various; a heredity factor, a morphological factor of brain tissues, a psychological factor and a biochemical factor (occidental medically) ; the 'Dam(痰) and Damhwa(痰火) caused by weakness of the internal organs and disturbance of the emotions(oriental medically). 5. Cerebral vascular dementia caused by loss of the certain cerebral neurons and oriental medically caused by obstruction of 'dam(痰)' or 'eo heul(瘀血)'. It is recommended that further study of many sided investigations, specially against a weakness of spiritual functions and a certain neurotoxin in the future.
각막윤부 결핍증 가토에 대한 생체내 자가 윤부각막상피세포 배양의 이식
이동원,박우찬,Dong-Won Lee,Woo-Chan Park 대한안과학회 2005 대한안과학회지 Vol.46 No.3
Purpose: To treat limbal stem cell deficiency, we investigated the epithelial characteristics in rabbits with total limbal stem cell deficiency (LSCD) after reconstruction with autologous limbal corneal epithelial cells in vivo expanded on amniotic membrane. Methods: The right eyes of 10 rabbits were rendered total LSCD, as verified by impression cytology. In the left eyes of 10 rabbits, in vivo limbal corneal epithelial cells culture was achieved. In group A (n=4), we evaluated the characteristics of the cultured limbal corneal epithelial cells and in group B (n=6) we evaluated the characteristics of the transplanted limbal corneal epithelial cells at postoperative 1, 2, and 4 weeks. Results: Successful epithelial growth was observed on amniotic membrane in all eyes of group A. Transplanted epithelial cells were well remained in five eyes of group B. The epithelial cells of group A and B were confirmed with corneal specificity by immunohistochemical staining (AK-2, AE-5). Conclusions: The corneal surface with unilateral total LSCD can be successfully reconstructed by transplantation with autologous limbal corneal epithelial cells in vivo expanded on amniotic membrane.
이동원,김부윤,정영우,Lee, Dong Won,Kim, Boo Yoon,Chung, Young Woo 영남수학회 2016 East Asian mathematical journal Vol.32 No.2
There are three subjects in the study. First, after investigating the development process of the method of infinite descent and the reduction to absurdity, we prove them to be equivalent each other. Second, we apply the method of infinite descent to some problems in textbook and compare it with the reduction to absurdity. Finally, we discuss on teaching proofs with the method of infinite descent.
화학기상응축공정에 의한 WS<sub>2</sub> 나노입자의 합성 및 특성평가
이동원,김주형,올레그토로츠코,윤중열,김병기,Lee, Dong-Won,Kim, Ju-Hyeong,Tolochko, O.,Yun, Jung-Yeul,Kim, Byung-Kee 한국분말야금학회 2008 한국분말재료학회지 (KPMI) Vol.15 No.4
Nano-sized tungsten disulfide ($WS_2$) powders were synthesized by chemical vapor condensation (CVC) process using tungsten carbonyl ($W(CO)_6$) as precursor and vaporized pure sulfur. Prior to the synthesis of tungsten disulfide nanoparticles, the pure tungsten nanoparticles were produced by same route to define the optimum synthesis parameters, which were then successfully applied to synthesize tungsten disulfide. The influence of experimental parameters on the phase and chemical composition as well as mean size of the particles for the produced pure tungsten and tungsten disulfide nanoparticles, were investigated.