CuO와 ZnO 첨가에 따른 NKN-BZT 세라믹스의 압전 특성
이승환,백상돈,이동현,이성갑,이영희,Lee, Seung-Hwan,Baek, Sang-Don,Lee, Dong-Hyun,Lee, Sung-Gap,Lee, Young-Hie 한국전기전자재료학회 2011 전기전자재료학회논문지 Vol.24 No.8
The lead-free $0.98(Na_{0.5},K_{0.5})NbO_3-0.02Ba(Zr_{0.52},Ti_{0.48})O_3$-(hereafter NKN-BZT) CuO, ZnO-doped ceramics were prepared using a conventional mixed oxide method. NKN-BZT ceramics doped CuO, ZnO have superior structural and electrical properties than pure NKN-BZT ceramics. For the NKN-BZT-ZnO ceramics sintered at $1,120^{\circ}C$, piezoelectric constant ($d_{33}$) of sample showed the optimum values of 172 pC/N. The $0.98(Na_{0.5},K_{0.5})NbO_3-0.02Ba(Zr_{0.52},Ti_{0.48})O_3$-ZnO ceramics are a promising candidate for lead-free piezoelectric materials.