Solubility of nitrogen in liquid iron, chromium and iron-chromium alloys has been measured by the sampling method under 1 atm N₂pressure. Experiments were carried out at the temperature range of 1829∼2205K and at the composition range of 0∼30.2%...
http://chineseinput.net/에서 pinyin(병음)방식으로 중국어를 변환할 수 있습니다.
변환된 중국어를 복사하여 사용하시면 됩니다.
https://www.riss.kr/link?id=A19592422
1985
Korean
530.000
학술저널
1-6(6쪽)
※ 저작자의 요청에 따라 해당 논문은 원문이 제공되지 않습니다.
0
상세조회0
다운로드다국어 초록 (Multilingual Abstract)
Solubility of nitrogen in liquid iron, chromium and iron-chromium alloys has been measured by the sampling method under 1 atm N₂pressure. Experiments were carried out at the temperature range of 1829∼2205K and at the composition range of 0∼30.2%...
Solubility of nitrogen in liquid iron, chromium and iron-chromium alloys has been measured by the sampling method under 1 atm N₂pressure. Experiments were carried out at the temperature range of 1829∼2205K and at the composition range of 0∼30.2% Cr.
Results obtained are as follows:
1) Nitrogen solubilities measured in pure iron and chromium were,
log(wt% N)_Fe = -341/T-1.157
log(wt% N)_cr = 2860/T-.701 respectively.
2) Interaction parameter in liquid Fe-Cr alloy was,
e^cr_N=-126/T+.0231
3) Enthalpy change of nitrogen solubility in Fe-Cr alloys was,
△H^cr_N=5600-2430(wt% Cr) J/g-atom N