In this study, in order to confirm the machining characteristics of AISI 1020 CD-Bar, cutting was performed after strength measurement, and surface roughness analysis was performed according to cutting conditions. Tensile strength was reduced by about...
In this study, in order to confirm the machining characteristics of AISI 1020 CD-Bar, cutting was performed after strength measurement, and surface roughness analysis was performed according to cutting conditions. Tensile strength was reduced by about 27.7% compared to AISI 1045 material, and Rockwell hardness HRC was reduced by 46.7%. The surface roughness measurement after cutting was divided into roughing, semi-finishing and finishing turning. In particular, in finishing machining, the best surface roughness was confirmed when the cutting speed was 150m/min and the depth of cut was 0.6mm based on the feed rate of 0.05mm/rev.