<P>PAA-grafted MWNTs containing POSS (POSS/PAA-grafted MWNTs) were synthesized by the simple mixing of octa(3-aminopropyl)octasils-esquioxane (POSS-NH3+) and PAA-grafted MWNTs via ionic interactions. The spherical aggregates of Pd nanoparticles ...
http://chineseinput.net/에서 pinyin(병음)방식으로 중국어를 변환할 수 있습니다.
변환된 중국어를 복사하여 사용하시면 됩니다.
https://www.riss.kr/link?id=A107735216
2017
-
SCOPUS,SCIE
학술저널
194-199(6쪽)
0
상세조회0
다운로드다국어 초록 (Multilingual Abstract)
<P>PAA-grafted MWNTs containing POSS (POSS/PAA-grafted MWNTs) were synthesized by the simple mixing of octa(3-aminopropyl)octasils-esquioxane (POSS-NH3+) and PAA-grafted MWNTs via ionic interactions. The spherical aggregates of Pd nanoparticles ...
<P>PAA-grafted MWNTs containing POSS (POSS/PAA-grafted MWNTs) were synthesized by the simple mixing of octa(3-aminopropyl)octasils-esquioxane (POSS-NH3+) and PAA-grafted MWNTs via ionic interactions. The spherical aggregates of Pd nanoparticles on the surface of POSS/PAA-grafted MWNTs (Pd-POSS/MWNTs) were produced with an average size of 10-20nm due to the effect of POSS-NH3+ used as a cubic linker physically attached to PAA-grafted MWNTs. The size of Pd-POSS/MWNTs was smaller than that of spherical aggregates of Pd nanoparticles prepared by only POSS-NH3+. The residual content of Pd-POSS/MWNTs is larger than that of POSS/PAA-grafted MWNTs because of the aggregates of Pd nanoparticles.</P>