<P><B>Abstract</B></P> <P>Deformation behavior and tensile properties of an austenitic Fe-24Mn-4Cr-0.5C high-manganese steel with different grain sizes were discussed in this study. Effective grain size including anneali...
http://chineseinput.net/에서 pinyin(병음)방식으로 중국어를 변환할 수 있습니다.
변환된 중국어를 복사하여 사용하시면 됩니다.
https://www.riss.kr/link?id=A107454584
2019
-
SCOPUS,SCIE
학술저널
334-343(10쪽)
0
상세조회0
다운로드다국어 초록 (Multilingual Abstract)
<P><B>Abstract</B></P> <P>Deformation behavior and tensile properties of an austenitic Fe-24Mn-4Cr-0.5C high-manganese steel with different grain sizes were discussed in this study. Effective grain size including anneali...
<P><B>Abstract</B></P> <P>Deformation behavior and tensile properties of an austenitic Fe-24Mn-4Cr-0.5C high-manganese steel with different grain sizes were discussed in this study. Effective grain size including annealing twins and stacking fault energy increased with increasing annealing temperature from 800 °C to 1200 °C. Room-temperature tensile test results indicated that the yield and tensile strengths increased, but the total elongation decreased with decreasing the effective grain size. According to electron back-scattered diffraction and transmission electron microscopy analyses, the deformed microstructure of all the specimens having stacking fault energy between 24.0 mJ/m<SUP>2</SUP> and 31.6 mJ/m<SUP>2</SUP> showed deformation twinning. However, the formation of the deformation twinning was suppressed with decreasing the grain size, resulting in different work hardening behaviors. Experimental and calculated twinning stress increased with decreasing the grain size because dislocation activity and the movement of partial dislocations required for form the deformation twinning were further inhibited by interaction of relatively high dislocation density in specimens with finer grain size.</P>
Laser weldability of cast and rolled high-entropy alloys for cryogenic applications