The optical magnetic sensor using Nd doped TiO<SUB>2</SUB> thin films
S. Harako,X. Zhao,F. Jing,S. Komuro,H. Aizawa,C. Nakayama,K. Otubo,T. Katsumata 제어로봇시스템학회 2008 제어로봇시스템학회 국제학술대회 논문집 Vol.2008 No.10
A TiO2:Nd formed on Si(100) substrate by laser ablation. The TiO2:Nd shows IR emissions at room temperature. The superconducting magnet was used for applied of a magnetic field. Magnetic field intensity was changed from 0.0 T (Tesla) to 8.0 T with PL measurement at room temperature. The sharp intense PL peak at 913.5 nm, 933.3 nm, 954.6 nm, 1093.7 nm and 1382.7 nm originating from the intra-4f shell transition in Nd<SUP>3+</SUP> ions was observed. The spectrum form change was according to the Zeeman effect with the rise of magnetic field intensity.